What is galvanic corrosion?
(V. brief summary) An electrochemical process were a more active metal in the galvanic series corrodes when connected to a more passive metal in the galvanic series . An electrolyte solution (i.e salt water) will cause electrons to flow from the anode to the cathode to cause corrosion- REDOX reaction
What are the parts of an electrochemical or ‘Galvanic cell’
Anode: The site were the metal is corroded (Undergoes oxidation reaction)
Cathode: Part of the same metal or surface or different metal surface which is protected from corrosion (undergoes reduction reaction)
Electrolyte solution: Corrosive medium which is electrically conductive
In a galvanic cell, which metal will corrode?
The metal with the more negative electrode potential (the more active metal/least noble) is likely to corrode whilst the other metal (the more passive metal/most noble) remains protected
When does galvanic corrosion occur?
When any dissimilar metals are connected in an electrolyte solution this will cause the anode to corrode.
Thus necessary to protect structural designs from corrosion, as corrosion weakens metals
How can Galvanic corrosion be prevented?
Do not connect dissimilar metals.
If this can’t be avoided
-electrically isolate one from another with rubber etc
-make the anode large and the cathode small
-eliminate the electrolyte
-make anode easily replaceable