Common material with an endurance limit (fatigue cracking cannot occur below this stress level)
CS
Subject to temper – embrittlement
Low Chromes
Common material without an endurance limit
Aust. SS
Subject to chloride stress – corrosion cracking
300 SS
Subject to polytheonic Acid stress – corrosion cracking
Sensitized 300 SS
P-#’s Allowed to use pre-heat in lieu of PWHT
P1 and P3
P-#’s Allowed to use controlled Deposition in lieu of PWHT
P1, P3, and P4