SPLIT PATTERNS
the original patter is divided along a suitable plane for separate use in the COPE and DRAG. COPE CAVITY and DRAG CAVITY
MATCH PATTERN OR PLATES
Solves misalignment issues for split patters by passing LOCKING PINS through holes in the MATCH PLATES
CORES definition
Create passageways, while denying access to molten metal
What are CORES made out of
Composite material consisting of SAND bonded together with THERMOSETTING RESIN such as UREA OR PHENOL FORMALDEHYDE
CORE PRINTS
generate indentations in the cavity wall for the core. Lets the workers know where to place core.
CHAPLET
supports one end of the core until it becomes fully surrounded by metal
CASTING DEFECTS/ FLAWS
NDT
Non Destructive Method
What is the solution to a COLD SHUT?
DYE PENETRANT
What is the solution to MISMATCH?
MATCH PLATES